Bimetallic Conical Twin Screw

Zhoushan Nanhaiya ke moetsi ea ka sehloohong oa Bimetallic conical twin screw naheng ea China ka lilemo tse fetang 20. Re fana ka tharollo ea sebaka se le seng masimong a amanang le polasetiki bakeng sa likhoebo tsa lefats'e. OEM ODM e tšehetsoa.

Zhoushan Nanhaiya ke moetsi ea ka sehloohong oa li-screw barrel Chaena ka lilemo tse fetang 20. Re fana ka tharollo ea sebaka se le seng masimong a amanang le polasetiki bakeng sa likhoebo tsa lefats'e. OEM ODM e tšehetsoa.

Bimetallic Conical Twin ScrewBimetallic Conical Twin Screw

Ke hobane'ng ha u khetha Nanhaiya?

1. Lintho tse tala tsa boleng bo holimo

Re sebelisa lisebelisoa tse tala tsa boleng bo holimo tse rekoang ka kotloloho ho litsila tsa tšepe, khetha tšepe ea boemo bo holimo, eo, ka ho forging le extrusion, e fihlelang boima bo betere le ho tiea.

2. E tsoetseng pele Bimetallic Craft

Re sebelisa motsoako oa nickel-based alloy + tungsten alloy e tsoang kantle ho naha. Bolelele ba motsoako o feta 400mm, 'me botebo ke 2 - 3mm. Alloy hardness e ka fihla HRC58-65. Alloy e ka etsoa ka mokhoa o ikhethileng ho latela litlhoko tsa bareki ho fihlela moaparo o betere le ho hanyetsa kutu, ka hona ho lelefatsa bophelo ba ts'ebeletso ea screw le barrel.

3. Phano e potlakileng

Bakeng sa li-screw tsa mofuta o tloaelehileng, re thehile sistimi e hlophisitsoeng ea thepa ho fihlela thomello e potlakileng nakong ea lihora tse 24-48; bakeng sa lihlahisoa tse ikhethileng, re itlama ho potoloha matsatsi a 30-40. Bareki ba ka boloka tlaleho ea tsoelo-pele ea odara ea nako ea 'nete ka lintlafatso tse nakong.

4. Tšebeletso ea lihora tse 24 ka mor'a thekiso

Re fana ka lits'ebeletso tsa bophelo bohle ka mor'a thekiso, ho kenyeletsoa tataiso ea ho kenya, ho rarolla mathata, le likhothaletso tsa ka mehla tsa ho lokisa. Sehlopha sa rona sa kamora ho rekisa se fana ka karabelo ea lihora tse 24 ho netefatsa tharollo e potlakileng ea litaba tsa bareki le ho fokotsa tahlehelo ea nako ea ho theoha haholo.

5. Excellent Litšenyehelo-ts'ebetso

Bakeng sa lihlahisoa tsa boleng bo tšoanang, re hlōlisana ka theko; bakeng sa lihlahisoa ka theko e tšoanang, re ipabola ka boleng. Nanhaiya Screws e ithorisa ka tšebeliso e ntle ea litšenyehelo, e ba etsa khetho ea hau e nepahetseng.

Bimetallic conical twin screw

Melemo ea mantlha ea li-screws tsa li-bimetallic conical twin li lutse ka mokhoa o babatsehang oa ho apara le ho hanyetsa ho bola, hammoho le bokhoni ba bona bo phahameng ba ho kopanya le ho etsa polasetiki bakeng sa thepa e thata haholo. Ho sa le joalo, li tsamaisana le lisebelisoa tsa extrusion tse nyane le tse mahareng, e leng se etsang hore e be likarolo tse ratoang bakeng sa ho sebetsana le thepa e tlatsitsoeng haholo le e senyang haholo.

Lisebelisoa tsa bona li shebane le maemo a thata haholo a ho sebetsana le thepa, haholo-holo masimong a nang le litlhoko tse phahameng tsa ho hanyetsa ho roala li-screw le bokhoni ba ho kopanya:

Phetoho ea Plastiki e Fetotsoeng

Tse kang khalase ea fiber-reinforced PP/PA (lisebelisoa tsa likarolo tsa likoloi) le PE / PVC e tletseng liminerale (lisebelisoa tsa liphaephe le litlaleho). E ka rarolla bothata ba ho roala ha li-screws tse bakiloeng ke lisebelisoa tse tlatsitsoeng haholo, ha e ntse e netefatsa ho hasana ha junifomo ea li-agent tse matlafatsang.

PVC le Corrosive Material Processing

Ho kenyeletsoa litlaleho tsa PVC-U, lipeipi tsa phepelo ea metsi tsa PVC-C, le lihlahisoa tsa fluoropolymer (mohlala, PVDF). Thepa ea bimetallic e ka hanela kutu ho tsoa ho hydrogen chloride e hlahisoang ke ho bola ha PVC, ho thibela mafome a screw ho ama boleng ba sehlahisoa.

Masterbatch le Functional Masterbatch Manufacturing

E sebelisoa bakeng sa granulation ea extrusion ea masterbatches a mebala e phahameng ea concentration (pigment content> 30%), masterbatches e thibelang malakabe, le li-antibacterial masterbatches. Bokhoni ba eona bo matla ba ho kopanya bo tiisa ho qhalakanngoa ha junifomo ea li-additives tse sebetsang, ho qoba matheba a mebala kapa ts'ebetso e sa tšoaneng ho lihlahisoa tse felileng.

Recycled Plastic Regeneration Processing

E sebetsana le lipolasetiki tsa litšila tse nang le litšila tse ngata (joalo ka lisebelisoa tse pshatlehileng tse tsoang ka har'a likhalase tsa lisebelisoa tsa lapeng le lisebelisoa tse sebelisoang hape ka likoloi). Ho hanyetsa ho roala ha thepa ea bimetallic ho ka sebetsana ka katleho le ho apara ho bakoang ke litšila, ha ho ntse ho ntlafatsa boleng ba ho qhibiliha ha thepa e tsosolositsoeng ka polasetiki e sebetsang hantle.

Tekheniki parameter 

Lintho tse bonahalang

38CrMoAlA

Boima ba ho kokobetsa

HB260-290

Nitriding hardness

HV900-1100    

Ho teba ha nitriding

0.5-0.8mm

Nitriding brittleness

≤ sehlopha sa 1   

Bokhoakhoa ba bokaholimo

Ra0.4   

Ho otloloha

0.015mm/m  

Ho thatafala ha Bimetal

HRC56-65

Botebo ba Bimetal

2.0-3.0mm  

Litlhaloso tsa Conical Twin Screw le Barrel

Φ 45/Φ 90

Φ 45/Φ 100

Φ 51/Φ 105

Φ 55/Φ 110

Φ 58/Φ 124

Φ 60/Φ 125

Φ 65/Φ 120

Φ 65/Φ 132

Φ 68/Φ 143

Φ 75/Φ 150

Φ 80/Φ 143

Φ 80/Φ 156

Φ 80/Φ 172

Φ 92/Φ 188

Φ 105/Φ 216

Φ 110/Φ 220

Bimetallic Conical Twin ScrewBimetallic Conical Twin ScrewBimetallic Conical Twin Screw
Bimetallic Conical Twin ScrewBimetallic Conical Twin ScrewBimetallic Conical Twin Screw
Bimetallic Conical Twin ScrewBimetallic Conical Twin Screw
Bimetallic Conical Twin ScrewBimetallic Conical Twin Screw
Romela Lipatlisiso
Contact Info
Rea u amohela webosaeteng ea rona! Bakeng sa lipotso mabapi le lihlahisoa tsa rona kapa lethathamo la litheko, ka kopo re siele lengolo-tsoibila la hau mme re tla ikopanya le rona nakong ea lihora tse 24.
X
Re sebelisa li-cookies ho u fa boiphihlelo bo betere ba ho bala, ho sekaseka sephethephethe sa sebaka sa marang-rang le ho iketsetsa litaba tsa hau. Ka ho sebelisa sebaka sena sa marang-rang, u lumellana le tšebeliso ea rona ea li-cookies. leano la lekunutu
HanaAmohela