Super Wear-Resistant One Screw
  • Super Wear-Resistant One ScrewSuper Wear-Resistant One Screw

Super Wear-Resistant One Screw

Khanyetso e ikhethang ea ho apara e qala ka Super Wear-Resistant Single Screw ea boleng bo holimo. Re khetha premium nitrided steel (e kang 38CrMoAlA) ho etsa bonnete ba hore motheo o matla ebile o tšoarella, o fana ka motheo o tiileng bakeng sa ho matlafatsa holim'a metsi.Fana ka mefuta e mengata ea litlhophiso tse sa senyeheng, ho tloha ho classic deep ion nitriding ho ea holimo-ea-line-motsoako oa litšepe tse peli.
Lintlha: 5.0
(Palo ea Lintlha: 1)

Lihlahisoa tsa lihlahisoa

Paramethara

Lintlha

Screw Diameter

Litlhaloso tse tloaelehileng li kenyelletsa 35mm, 45mm, 65mm, 75mm, 85mm, 90mm, joalo-joalo. Ka mohlala, ha ho sebetsa liphaephe tsa PVC, sekoti sa 65mm se sebelisoa haholo ha se finyella tekanyo e ntle pakeng tsa tlhahiso le matla a matla.

Length-to-Diameter Ratio (L/D Ratio)

Ka kakaretso e fapana ho tloha ho 20:1 ho isa ho 30:1. Bakeng sa lipolasetiki tse mamellang mocheso joalo ka PVC, karolelano ea L/D hangata e lipakeng tsa 20:1 le 25:1. Sena se tiisa hore polasetiki e lekaneng ha e ntse e fokotsa nako ea ho lula ha thepa ka har'a barrel ho fokotsa kotsi ea ho bola.

Compression ratio

Hangata e oela pakeng tsa 3.5:1 le 4.5:1. Karolelano e kholo ea compression e thusa ho etsa polasetiki e felletseng le ho kopana ha lisebelisoa tsa PVC.

Screw Channel botebo

The screw channel e batla e sa teba, haholo-holo karolong ea metering. Moralo ona o fokotsa nako ea ho lula ha thepa mme o fokotsa monyetla oa ho bola.

Palo ea Libaka tsa ho futhumatsa le ho futhumatsa

E fapana ho ipapisitsoe le bophara ba screw le litlhaloso tsa lisebelisoa, hangata ho tloha ho libaka tse 5 ho isa ho tse 6. Mohlala, extruder e nang le sekerufu se le seng se bophara ba 65mm se ka ba le libaka tse 6 tsa ho futhumatsa le ho pholisa ho nolofalletsa taolo e nepahetseng ea mocheso karolong ka 'ngoe.

Screw Speed

Lebelo la lebelo le hloka ho lokisoa ho ea ka bophara bo khethehileng ba screw diameter le litlhoko tsa tlhahiso. Bakeng sa sekoti sa φ65mm, ha ho hlahisa liphaephe tse nang le botenya ba lerako la 3mm, lebelo le khothalletsoang le laoloa ka har'a sebaka sa 25-35rpm.

Drive Power

E amanang le bophara ba screw le tlhahiso. Ka mohlala, extruder e nang le sekoti se le seng se nang le bophara ba 65mm screw hangata e na le matla a ho khanna a 45-90kw.

Mocheso oa ho sebetsa

Thempereichara ea karolo ea ho fepa hangata ke 160-170 ℃, karolo ea ho qhibiliha ke 180-190 ℃, 'me karolo ea hlooho ea lefu ke 175-185 ℃.

Sehlahisoa Tšobotsi Le Kopo

1. Double-metal Super Wear-Resistant Single Screw, Sebelisa tšepe e matla a phahameng joalo ka thepa ea motheo,38CrMoAlA, SACM645, 42CrMo joalo-joalo, karolo e ka tlase ea tšepe e entsoeng ka tšepe e phahameng.

2. Alloy super wear-resistance barrel, masoba a ka hare a carbon steel substrate a entsoe ka centrifugally kapa alloy e sa senyeheng,Bothata ba alloy bo feta HRC 60.

3. Bakeng sa maemo a khethehileng a ho apara ka holimo, re fana ka tiiso ea bophelo ba sehlahisoa.

Super wear-resistant barrel screw, e loketseng li-plastic fiber reinforced plastics (GF), e nang le calcium carbonate, talc powder, lisebelisoa tse tsosolositsoeng tse sebetsang hantle, litšila tse tsosolositsoeng, le lipolasetiki tse senyang, joalo-joalo.

4.E sebetsa ho lisebelisoa tse ngata,GFPA GFPBT GFPPS GFPP GFPOM CF PPS...

Super Wear-Resistant Single ScrewSuper Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw

Lintlha tsa Tlhahiso

1. PTA e sebelisetsoa ho etsa welding ka holimo le mahlakoreng a likhoele tsa screw, e leng libaka tse atisang ho roala.

2. Ion nitriding e fella ka microstructure e teteaneng le boima bo phahameng (ho fihlela ho HV1000-1200), e nang le deformation e fokolang.

3.Bokaholimo ba sekoti se fafatsoa kapa se koahetsoe ka tungsten carbide (WC), li-alloys tse thehiloeng ho nickel, joalo-joalo Bophelo ba tšebeletso bo ka eketsoa ka makhetlo a 3 ho isa ho a 8.

Super Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw
Super Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw
Romela Lipatlisiso
Contact Info
Rea u amohela webosaeteng ea rona! Bakeng sa lipotso mabapi le lihlahisoa tsa rona kapa lethathamo la litheko, ka kopo re siele lengolo-tsoibila la hau mme re tla ikopanya le rona nakong ea lihora tse 24.
Lintlha:
5.0
X
Re sebelisa li-cookies ho u fa boiphihlelo bo betere ba ho bala, ho sekaseka sephethephethe sa sebaka sa marang-rang le ho iketsetsa litaba tsa hau. Ka ho sebelisa sebaka sena sa marang-rang, u lumellana le tšebeliso ea rona ea li-cookies. leano la lekunutu
HanaAmohela